Time | Paper ID | Title / Authors | Keywords | Topic code | Ack. number |
SY-77 [Symposium of Division of Materials and Interfaces] Cutting Edge of Innovative Materials and Advanced Interfacial Phenomena (Oral Session) |
(9:20–10:40) (Chair: Yamamoto Tetsuya) |
9:20– 9:40 | DG302 | Two-stage microwave irradiation method for maintaining interface modification characteristics
| Microwave interfacial tension Refractive index
| SY-77 | 70 |
9:40– 10:00 | DG303 | One-step synthesis of submicron-sized silica coated FeNi particles via spray pyrolysis
| Spray pyrolysis FeNi core-shell particle
| SY-77 | 587 |
10:00– 10:20 | DG304 | Synthesis of titanosilicate nanoparticles using a precursor unit to introduce high concentration of Ti(IV) species
| Titanosilicate nanoparticle precursor
| SY-77 | 390 |
10:20– 10:40 | DG305 | Synthesis of porous catalyst particles by spray pyrolysis and three-dimensional reconstruction
| Porous particle Gas adsorption rate 3D structure analysis
| SY-77 | 350 |
(11:00–12:00) (Chair: Hirano Tomoyuki) |
11:00– 11:20 | DG307 | Nanosizing of Polymeric Particles using a 3D Micro-Network Reactor
| Polymer Nano Particle 3D Micro-Network Reactor Melamine Foam
| SY-77 | 22 |
11:20– 11:40 | DG308 | Investigation of mechanical properties of stretchable latex films prepared from elastomer microspheres
| latex films mechanical properties colloids
| SY-77 | 521 |
11:40– 12:00 | DG309 | Fabrication of CeO2 nanoparticle loaded plastic scintillator by supercritical hydrothermal synthesis
(Tohoku U.) *(Stu)Komatsuzaki Shusuke, (Shizuoka U.) Koshimizu Masanori, (Tohoku U.) Fujimoto Yutaka, (Stu)Watanabe Akito, Satou Atsusi, (Tohoku U. AIMR) (Reg)Yoko Akira, (Tohoku U. NICHe) (Reg)Seong Gimyeong, (Tohoku U. IMRAM) (Reg)Tomai Takaaki, (Tohoku U. AIMR) (Reg)Adschiri Tadafumi, (KEK) Kishimoto Shunji, (Tohoku U.) Asai Keisuke | nanoparticles cerium scintillator
| SY-77 | 668 |
(13:00–13:40) (Chair: Tanaka Hideki) |
13:00– 13:40 | DG313 | [Invited lecture] Development of sealing glass for SOFC
| SOFC sealing glass bonding strength
| SY-77 | 169 |